The Morphology Evolution and Voiding of Solder Joints on QFN Central Pads with a Ni/Au Finish
Published: |
October 18, 2012 |
Author: |
Julie Silk, Jianbiao Pan, Mike Powers |
Abstract: |
First published in the 2012 IPC APEX EXPO technical conference proceedings. In this paper, we report on a comprehensive study regarding the morphology evolution and voiding of SnAgCu solder joints on the central pad of two different packages – QFN and an Agilent package called TOPS – on PCBs with a Ni/Au surface finish.... |
You must be a registered user to talk back to us. |
Company Information:
More articles from Agilent Technologies, Inc. »
- Dec 17, 2015 - Good Product Quality Comes From Good Design for Test Strategies
- Aug 13, 2015 - Pad Cratering Susceptibility Testing with Acoustic Emission
- Aug 29, 2013 - Effect of Gold Content on the Microstructural Evolution of SAC305 Solder Joints Under Isothermal Aging
- Feb 14, 2013 - Boundary Scan Advanced Diagnostic Methods
- Sep 20, 2012 - Evaluation of Laminates in Pb-free HASL Process and Pb-free Assembly Environment
- See all SMT / PCB technical articles from Agilent Technologies, Inc. »
More SMT / PCB assembly technical articles »
- Apr 11, 2022 - iNEMI Webinar 07.07.2021 - PCB Cleaning | ZESTRON Americas
- Jan 28, 2022 - Open Radio Unit White Box 5G | Whizz Systems
- Nov 10, 2021 - Understanding the Cleaning Process for Automatic Stencil Printers | ITW EAE
- Oct 20, 2021 - PCB Surface Finishes & The Cleaning Process - A Compatibility Study | ZESTRON Americas
- Oct 06, 2021 - Cleaning Before Conformal Coating | ZESTRON Americas
- Browse Technical Library »
The Morphology Evolution and Voiding of Solder Joints on QFN Central Pads with a Ni/Au Finish article has been viewed 633 times