Abstract: |
With the miniaturization of electronic device, Land Grid Array (LGA) or QFN has been widely used in consumer electronic products. However there is only 20-30 microns gap left between LGA and the substrate, it is very difficult for capillary underfill to flow into the large LGA component at room temperature. Insufficient underfilling will lead to the loss of quality control and the poor reliability issue. In order to resolve these issues, a room temperature fast flow reworkable underfill has been successfully developed with excellent flowability. The underfill can flow into 20 microns gap and complete the flow of 15mm distance for about 30 seconds at room temperature. The curing behavior, storage, thermal cycling performance and reworkability will be discussed in details in this paper.... |
You must be a registered user to talk back to us. |
Company Information:
More articles from YINCAE Advanced Materials, LLC. »
- Apr 05, 2018 - High Reliability and High Throughput Ball Bumping Process Solution – Solder Joint Encapsulant Adhesives
- Oct 16, 2017 - High Reliability and High Temperature Application Solution - Solder Joint Encapsulant Paste
- Nov 17, 2016 - A High Thermal Conductive Solderable Adhesive
- Jan 12, 2016 - A Low Cost Manufacturing Solution - Low Temperature Super-Fast Cure and Flow Reworkable Underfill
- Jan 12, 2016 - A Room Temperature Stable and Jetable Solder Joint Encapsulant Adhesive - Capillary Underfill Replacement
- See all SMT / PCB technical articles from YINCAE Advanced Materials, LLC. »
More SMT / PCB assembly technical articles »
- Apr 11, 2022 - iNEMI Webinar 07.07.2021 - PCB Cleaning | ZESTRON Americas
- Jan 28, 2022 - Open Radio Unit White Box 5G | Whizz Systems
- Nov 10, 2021 - Understanding the Cleaning Process for Automatic Stencil Printers | ITW EAE
- Oct 20, 2021 - PCB Surface Finishes & The Cleaning Process - A Compatibility Study | ZESTRON Americas
- Oct 06, 2021 - Cleaning Before Conformal Coating | ZESTRON Americas
- Browse Technical Library »
Room Temperature Fast Flow Reworkable Underfill For LGA article has been viewed 916 times